  • 1, stress relief before plating where the maximum tensile strength is greater than 1034Mpa key and important parts before plating should be at 200±10℃ stress relief for more than 1 hours, carburizing or surface quenching parts should be at 140±10℃ stress relief for more than 5 hours.