  • If the zinc coating is good, but when the light comes out in 3% nitric acid, there is a dark shadow on the coating, and the film is brown when passivation occurs, which may be caused by foreign metal impurities such as copper or lead in the galvanized liquid. When there is a problem in the process of galvanizing, check the temperature and current density first, and then measure and adjust the content of zinc and sodium hydroxide in the bath through the analysis of the bath. Whether DPE levels are low can be determined by Hull cell test.

  • The temperature of large roll galvanized wire should be controlled at 30 to 50℃ during electroplating. Because the chloride ions in the bath are very corrosive, quartz glass heaters are generally used. Continuous production does not need heating, but needs cooling. Cooling can be in the groove side row thin wall plastic pipe, through the flow of tap water cooling, can also be used as a titanium pipe temperature control device.