  • Poor pretreatment before electroplating; Bath temperature is too low; Poor quality additives or excessive additives and organic impurities can cause poor bonding. The quality of the additive also has an effect on coating foaming. Some additives react incompletely during synthesis and continue to polymerize during long-term storage or use. The additive tends to distort the lattice and create stress, causing the coating to blister.

  • In addition to these reasons, we should also pay attention to the tooling and process must be stable, and regular testing should be done to ensure the uniformity of galvanized layer.