  • The methods to control the thickness of galvanizing are as follows: you can slow down the lifting speed of the workpiece, control the time of galvanizing as far as possible, add the appropriate amount of thinning alloy, reduce the thickness, and improve the temperature of hot-dip galvanizing. But consider the zinc pot, iron pot should not exceed 480 degrees, ceramic pot can be 530 degrees, which can reduce the time of zinc immersion.


  • Post time: 29-09-22
  • Generally, galvanized wire used for welding is required to have a certain hardness. After acceptance of galvanized wire, the first thing to do is to feel the hand, and the other thing is to test on the machine. Because the average user does not have testing equipment, it is also very inconvenient to test on the machine. Use a micrometer to measure the diameter of galvanized wire evenly, and keep it about 0.02mm above and below the contract signing standard, with neat appearance, no leakage plating and no mess.