  • If the coating roughness is not caused by the above reasons, it may be caused by impurities in the plating solution. Can take a small amount of electroplating solution, after filtration test, then take a small amount of electroplating solution, after zinc powder treatment test, check the problem is caused by solid particles or copper, lead and other foreign metal impurities. Test them one by one and it’s not hard to find the cause of the problem. Galvanized iron wire coating foaming, binding force is not good.

  • More network is the application of the stone cage net, stone cage net because it is used in water conservancy engineering more, so the anticorrosion performance requirements for wire is relatively high, so the general use of zinc aluminum alloy wire or high galvanized wire. Common wire diameter has 2.0mm, 2.2mm, 2.5,mm, 2.7mm and so on.