  • Cold galvanized is in the plating tank through the current unidirectional zinc gradually plated on the metal surface, production speed is slow, uniform coating, thin thickness, usually only 3-15 microns, bright appearance, poor corrosion resistance, generally a few months will rust. Compared with electrogalvanizing, hot galvanizing has lower production cost and less impact on the environment than electroplating.

  • The key and important parts with tensile strength greater than 1034Mpa should be relieved of stress at 200±10℃ for more than 1 hour before plating, and the carburized or surface hardened parts should be relieved of stress at 140±10℃ for more than 5 hours. The cleaning agent used for cleaning shall have no effect on the binding force of the coating and no corrosion on the substrate. Acid activation Acid activation solution should be able to remove corrosion products and oxide film (skin) on the surface of parts without excessive corrosion on the matrix.

  • Post time: 02-06-22
  • Latest articles

    Links