  • A. When the thickness of the plating is 3-4 mm, the zinc adhesion should be less than 460g/m, that is, the average thickness of the zinc layer is not less than 65 microns.

  • There is no adhesion test of powder spraying or fluorocarbon spraying on packaged galvanized wire, but there are two points for reference: first, in sealed or air-free environment, non-metallic volatiles can corrode zinc coating; Second, zinc at higher than 230 degrees (c) will cause the matrix metal brittle. And powder spraying and fluorocarbon spraying are to be baked at a higher temperature and in a sealed environment, causing rapid corrosion of zinc, resulting in loose corrosion film resulting in coating adhesion decline, and even lead to (matrix) steel wire brittle situation may exist.

  • The most obvious gap in a short period of time is the cross section of this piece, hot dip galvanized wire because it is surface anti-corrosion treatment, so in the cross section of this piece will appear rust, and stainless steel wire because the internal raw materials and surface raw materials are consistent, so there is no such situation.

  • Latest articles

    Links