  • There is no adhesion test of powder spraying or fluorocarbon spraying on packaged galvanized wire, but there are two points for reference: first, in sealed or air-free environment, non-metallic volatiles can corrode zinc coating; Second, zinc at higher than 230 degrees (c) will cause the matrix metal brittle. And powder spraying and fluorocarbon spraying are to be baked at a higher temperature and in a sealed environment, causing rapid corrosion of zinc, resulting in loose corrosion film resulting in coating adhesion decline, and even lead to (matrix) steel wire brittle situation may exist.

  • The use of spring in a specific environment, there will be some special requirements for steel wire, such as: the use of spring in corrosive media, must have good corrosion resistance function. Precision instruments used in the spring, should have long-term stability and sensitivity, temperature coefficient to be low, high quality elements, after effect to be small, elastic modulus to be stable.