mine screen mesh

Latest articles



Popular articles

  • D, coating adhesion; The zinc layer of the plating parts should be firmly combined with the base metal with sufficient adhesion strength, and will not fall off or bulge after the hammer test.

  • Poor pretreatment before plating; Bath temperature is too low; Poor quality of additives or too many additives and organic impurities will cause poor bonding. The quality of additives also has an effect on coating foaming. Some additives react incompletely during synthesis and continue to polymerize during long-term storage or use. The additive tends to distort the crystal lattice and cause stress, causing the coating to bubble.