  • There is no adhesion test of powder spraying or fluorocarbon spraying on packaged galvanized wire, but there are two points for reference: first, in sealed or air-free environment, non-metallic volatiles can corrode zinc coating; Second, zinc at higher than 230 degrees (c) will cause the matrix metal brittle. And powder spraying and fluorocarbon spraying are to be baked at a higher temperature and in a sealed environment, causing rapid corrosion of zinc, resulting in loose corrosion film resulting in coating adhesion decline, and even lead to (matrix) steel wire brittle situation may exist.

  • Production technology: Through the excellent low carbon steel rod drawing forming, pickling rust removal, high temperature annealing, hot dip galvanizing. Cooling and other 5 operation processes refined. Galvanized wire characteristics: good resistance and elasticity, strong corrosion resistance.