  • Pressure lock steel grid plate is at each intersection of bearing flat steel and horizontal bar, the horizontal bar is pressed into bearing flat steel or pre-slotted bearing flat steel through the pressure, the fixed steel grid plate, called pressure lock steel grid plate. The cross bar of the pressure lock steel grid plate is usually flat steel.

  • There is no adhesion test of powder spraying or fluorocarbon spraying on packaged galvanized wire, but there are two points for reference: first, in sealed or air-free environment, non-metallic volatiles can corrode zinc coating; Second, zinc at higher than 230 degrees (c) will cause the matrix metal brittle. And powder spraying and fluorocarbon spraying are to be baked at a higher temperature and in a sealed environment, causing rapid corrosion of zinc, resulting in loose corrosion film resulting in coating adhesion decline, and even lead to (matrix) steel wire brittle situation may exist.