black wire crate

Latest articles



  • 2, see if solder joint is firm, net width on both sides of whether level off, the wire have broken wire phenomena (note: net length is the length of the wire), welded wire mesh of the solder joint is normal after precise voltage debugging, welding of welded wire mesh with graphite, strong, and the net width on both sides of the cutting time is according to the broken wire knife to ensure smooth on both sides, There will be no leakage cutting on both sides of the protrusion of the wire is not cut off the phenomenon, the wire is broken, because the wire is not used up even if the column hole is blocked by the wire can not enter the normal cause, such as broken phenomenon can appear on the surface of the electric welding network lack of a wire.

  • However, because the bath contains highly toxic cyanide, the gas escaping from the electroplating process will do great harm to the health of workers, and its waste water must be strictly treated before discharge. Galvanized iron wire has good anti-corrosion and anti-rust ability, so it can be used in some outdoor guardrails or fences, especially on handicrafts, which are also of great use. Galvanized iron wire is not easy to rust and oxidation on the surface.

  • Galvanized iron wire is divided into hot galvanized wire and cold galvanized wire, using low carbon steel wire processing, after drawing molding, pickling rust removal, high temperature annealing, hot galvanized, cooling and other processes. It has good toughness and elasticity, and the amount of zinc can reach 300 grams/square meter. It has the characteristics of thick galvanized layer and strong corrosion resistance. Galvanized iron wire can be cut off in the construction of the tie wire, the length of 20cm, 30cm and 40cm, can be cut off according to requirements.

  • Packaging and binding electric galvanized wire is in the state of liquid zinc, after messy physical and chemical effects, not only on the steel plating thicker pure zinc layer, and also generate a zinc – iron alloy layer. This plating method not only has the corrosion resistance characteristics of galvanized wire, but also has a zinc-iron alloy layer. It also has strong corrosion resistance that can not be compared with galvanizing. Therefore, this plating method is especially suitable for all kinds of strong acid, alkali fog and other strong corrosion environment.

  • Links