window aluminium mesh

Latest articles



  • Galvanized wire to galvanized uniform, a body is now its cross section, the second is the longitudinal uniformity. In the actual operation process, such as the jitter of steel wire, the surface of the pot scum and other reasons will cause galvanized wire surface galvanized layer accumulation, should try to solve the problem.

  • No less than 5 disks should be extracted from each inspection lot for diameter error inspection. 1 point of steel wire should be extracted from each disk to measure steel wire diameter, and the actual diameter of steel wire at this point should be taken as the average value of the two vertical directions. The diameter error of cold-drawn low carbon steel wire should conform to the rules in the table below. The unqualified inspection batches shall be checked one by one, and the qualified batches can be used for engineering.