  • D, coating adhesion; The zinc layer of the plating parts should be firmly combined with the base metal with sufficient adhesion strength, and will not fall off or bulge after the hammer test.

  • The duration of the protective effect of galvanized layer on large roll galvanized wire is closely related to the coating thickness. Generally speaking, in the dry main gas and indoor use, the thickness of galvanized layer only 6-12μm, and in the environment is more severe conditions, galvanized layer thickness needs 20μm “to be up to 50μm”. Therefore, the influence of environment should be considered when choosing the thickness of galvanized layer.