  • 5, the concentration of plating aid can not be too high, which is a factor that can not be ignored to reduce zinc consumption. The concentration of plating aid should not be too high. The galvanized line must be added with ammonium chloride and zinc chloride according to the data of laboratory analysis, and the specific gravity of the composite solution should be controlled within the range of 50~80g/L. If ammonium chloride or zinc chloride is arbitrarily added without the results of laboratory analysis, it should be criticized and educated, and economic treatment should be given if necessary.

  • Decorative hook mesh size width generally does not span 2 meters. Generally, the length does not span 4m. The length of 2 meters is difficult for workers, and the second is that the galvanized plating is not good. It can reach up to six meters in length, but it doesn’t cross six meters. Generally, the price will increase significantly after 4 meters.