fencing iron wire

Latest articles



Popular articles

  • barbed

  • barbed

  • If the zinc coating is good, but in 3% nitric acid when the light, the coating has dark shadow, passivation occurs when the film is brown, may be caused by foreign metal impurities such as copper or lead in the galvanizing liquid. When problems occur in the process of galvanizing large coil galvanized wire, the temperature and current density are checked first, and then the content of zinc and sodium hydroxide in the plating solution is measured and adjusted through the analysis of the plating solution. Whether DPE content is low can be determined by hull cell test.

  • Galvanized hexagonal mesh is a kind of galvanized metal wire mesh, the mesh shape is hexagonal.

  • Latest articles

    Links