  • blade

  • If the zinc coating is good, but in 3% nitric acid when the light, the coating has dark shadow, passivation occurs when the film is brown, may be caused by foreign metal impurities such as copper or lead in the galvanizing liquid. When problems occur in the process of galvanizing large coil galvanized wire, the temperature and current density are checked first, and then the content of zinc and sodium hydroxide in the plating solution is measured and adjusted through the analysis of the plating solution. Whether DPE content is low can be determined by hull cell test.

  • The production of large rolls of galvanized wire iron can be divided into two categories, is directly from the iron ore after iron stroke exercise out of the metal, the composition of the ore is iron oxide, silica and other miscellaneous stone.