  • When the zinc layer is seriously damaged and endangers the iron matrix, the zinc will produce electrochemical protection on the matrix, the standard potential of zinc is -0.76V and the standard potential of iron is -0.44V. When zinc and iron form microbatteries, the zinc will be dissolved as the anode, and the iron will be protected as the cathode. Obviously, the atmospheric corrosion resistance of hot dip galvanizing is better than that of electric galvanizing.

  • welding

  • Galvanized wire is immersed in heated molten zinc, the production speed is fast, the coating is thick but uneven. The thickness of 45 microns allowed by the market, the color is dark, the consumption of zinc metal is more, and the matrix metal is formed into an infiltration layer, and the corrosion resistance is good. The hot dip galvanizing can be maintained for decades in the outdoor environment.