  • If the zinc coating is good, but in 3% nitric acid when the light, the coating has dark shadow, passivation occurs when the film is brown, may be caused by foreign metal impurities such as copper or lead in the galvanizing liquid. When problems occur in the process of galvanizing large coil galvanized wire, the temperature and current density are checked first, and then the content of zinc and sodium hydroxide in the plating solution is measured and adjusted through the analysis of the plating solution. Whether DPE content is low can be determined by hull cell test.

  • When in use, wrap into a roll cage. First, its ventilation is good, conducive to the air drying of corn; Second, occupy a small space, convenient drying, good air permeability, light transmission; Third, beautiful and strong, reusable, cost-effective. And in the storage process, it is easy to cover in rain and snow weather to avoid the deterioration of corn mold.