Latest articles

  • 6, passivation to remove hydrogen parts should be passivation after the removal of hydrogen, passivation before the application of 1%H2SO4 or 1% hydrochloric acid activation 5~15s. Passivation shall be treated with colored chromate unless otherwise specified in the design drawings.

  • 1. Electroplating process control

  • Cooling can be in the groove close row of thin wall plastic pipe, through the flow of tap water for cooling, can also be used as a temperature control device titanium pipe. In the process of electroplating galvanized wire, it is necessary to stir the plating solution to obtain the composite coating with particles dispersing in the matrix metal. Stirring methods include mechanical stirring, air stirring, ultrasonic stirring, bath circulation, etc.