  • In this temperature range, the zinc solution is severely corroded to the workpiece and the zinc pot, and the iron is lost at 560 degrees Celsius to add obviously, and the zinc will be the iron substrate above 660 degrees Celsius, zinc slag will be added quickly, plating cannot be used. Therefore, electroplating is carried out in the range of 430~450 degrees Celsius.

  • The form of installation: in the top with the various cage tied together at least as wrapped stone cage net that combination closely not easy to use bad. If the local bandaging is appropriate, it can increase the stability of the structure. There are a lot of grid edge, if the stone cage net only hook in the cage edge and not prepared in the cage edge, even in loose.