anti climb welded mesh

Latest articles




  • Post time: 01-06-23

  • The size of the galvanized layer of galvanized iron wire is related to the anti-corrosion ability and application effect of galvanized wire. The thickness of the galvanized layer of the general standard galvanized wire products should be tested after the product is formed. There are three specific test methods. Weighing method and cross section microscopy method are destructive experimental methods, and magnetic method is a relatively rigorous non-destructive method, but the measurement steps and requirements are relatively high, so they are rarely used in specific applications. The first two methods are intuitive and common methods.

  • B. When the thickness of the plating is greater than 4 mm, the zinc adhesion should not be less than 610g/m, that is, the average thickness of the zinc layer should not be less than 86 microns.