  • 6, passivation to remove hydrogen parts should be passivation after the removal of hydrogen, passivation before the application of 1%H2SO4 or 1% hydrochloric acid activation 5~15s. Passivation shall be treated with colored chromate unless otherwise specified in the design drawings.

  •  

  • There is no adhesion test of powder spraying or fluorocarbon spraying on packaged galvanized wire, but there are two points for reference: first, in sealed or air-free environment, non-metallic volatiles can corrode zinc coating; Second, zinc at higher than 230 degrees (c) will cause the matrix metal brittle. And powder spraying and fluorocarbon spraying are to be baked at a higher temperature and in a sealed environment, causing rapid corrosion of zinc, resulting in loose corrosion film resulting in coating adhesion decline, and even lead to (matrix) steel wire brittle situation may exist.