Latest articles


  • Deoxygenation of boiling steel is incomplete, oxygen content is high, phosphorus and other impurities distribution is uneven, local overspending, aging sensitivity and cold brittle sensitivity are high, hot cracking tendency is added. If unqualified electrode is used, if the content of carbon and sulfur in the weld metal is too high, cracks will occur. For example, when factories use acidic electrodes to weld Q235-A steel, the high carbon fernoganese in the electrode coating will lead to thermal cracks in the weld.
  • The common specifications of small hexagonal net in production are: the width is 1.22m, and the commonly used width is generally 1m. In terms of length, the small hexagonal net basically has no limitation. 1-100 meters can be produced. The production diameter of small hexagonal mesh is generally No. 27 wire to No. 18 wire, and the aperture size is 0.95cm-5.08cm.