  • In addition, before the wire enters the zinc liquid, a layer of insulation material containing zinc oxide reducing agent can reduce the heat loss and zinc ash floating. When the zinc solution contains 0.002%-0.005% aluminum, the brightness of the zinc layer can be increased obviously, and excessive zinc ash can be prevented from oxidation on the surface of the zinc solution.

  • Zinc dipping time should be adjusted according to the thickness of wire diameter. The method of adjustment is to use the lead screw above the zinc pot, the length of the distance to the ceramic sinking roller. Thick wire diameter zinc dipping time should be long, fine wire diameter zinc dipping time should be short, zinc dipping length is in the range of 2~3.5m, which is also to reduce the zinc consumption of steel wire, is an aspect of maintaining the uniformity of zinc layer.